100mL Yttria Stabilized Zirconia Jar with Lid – Description:
Zirconium Dioxide Ceramic Specifications:
Density: 6.05 g/cm³
Water absorption: <0.05%
Firing temperature: 1550 °C
Hardness: 1350 HV
Flexural strength: 950 MPa
Compressive strength: 25 000 MPa
Fracture toughness: 6–8 MPa·m½
Thermal expansion coefficient: 9.5×10^-6 /°C
Alternate names for Yttria Stabilized Zirconia Jar: Yttria Stabilized Zirconia Grinding Jar (YSZ Grinding Jar), Zirconia Jar and Zirconium Oxide Jar.
The advantages of the Yttria Stabilized Zirconia Grinding Jar and Grinding Media include:
- High density
- High hardness and toughness, 60 times the hardness of standard steel
- High thermal expansion
- Low thermal conductivity
- Impact resistance
- High corrosion and wear resistance
100mL Yttria Stabilized Zirconia Jar with Lid Specifications:
|
TYP-MQ
|
TYP-GT
|
Capacity
|
100 mL
|
100 mL
|
Outer diameter
|
63 mm
|
68 mm
|
Height
|
63 mm
|
60 mm
|
Wall thickness
|
7 mm
|
7 mm
|
Lid thickness
|
7 mm
|
7 mm
|
The dimensions provided above serve as a reference only. Contact us for precise specifications or custom requests.
*Grinding media recommendation: When using a 100 mL YSZ jar, 100 pieces of 5 mm diameter balls or 16 pieces of 10 mm diameter balls are recommended.
100mL Yttria Stabilized Zirconia Jar with Lid Applications:
- YSZ grinding jars are used to mill materials into extremely fine powders for use in mineral processing, paints, pyrotechnics, ceramics and selective laser sintering.
- Zirconium dioxide jars and zirconium dioxide balls exhibit stability and possess high abrasion resistance, thereby preventing the inclusion of extraneous contaminants during milling in a ball mill.
100mL Yttria Stabilized Zirconia Jar with Lid Packaging:
SAM's zirconium dioxide grinding jars and YSZ grinding jars are carefully handled to minimise damage during storage and transport, thereby preserving the original quality of our products.
Safety Data Sheet (MSDS) for your reference!